PROFILE ENGINEERING / FORM STUDIO 1

Resin Profile Lab v7.26

Create custom Form Studio 1 print profiles for third-party resins — without manually configuring dozens of settings in PreForm.

Import a genuine factory FPS, enter your resin's recommended settings, and calculate an initial exposure profile. Compare, calibrate, and export when you're ready.

COMPATIBILITYForm Studio 1 .fps profiles only
IMPORTANTExperimental estimates. Verify inputs and calibrate before production.
Required hardware: Resin Tank Pro
When printing with third-party resins on the Form Studio 1, use the Resin Tank Pro. Do not attempt to print with an incompatible resin tank: the print may fail and using the wrong tank can damage the printer. Confirm that the correct tank is installed before starting any calibration or production print.
View compatible accessories in the Formlabs webshop ↗
Before you export: These are starting estimates calculated from the nominal 4.5 mW/cm² light intensity of the Anycubic Photon Mono M7 Max (adjustable below), not verified Studio 1 print settings. Check your resin-specific exposure time, layer thickness, irradiance and every other input before saving an FPS file. Incorrect values are likely to cause print failure, poor adhesion or damage. Import a genuine PreForm-exported FPS template and verify every output in PreForm. Formlabs: Using the Print Settings Editor (FPS import instructions) ↗

Step 1 · Import — Factory Studio 1 FPS

In PreForm, open the Print Settings Editor, select a factory Studio 1 resin profile, and enable Open Material before exporting. This ensures the imported custom profile appears under Open Material in Job Setup. Export the factory profile as an .fps file, then import it here. Formlabs: Using the Print Settings Editor ↗

Required before exporting the factory FPS: enable Open Material in PreForm.

No FPS template loaded. Only Form Studio 1 material profiles are accepted.

Step 2 · Configure — Source printer & resin

Enter the resin-specific exposure settings from your source slicer. The M7 Max defaults are examples only. Verify every value against your actual resin profile. Temperature: Operating Temperature is the resin temperature the printer attempts to maintain while printing. Start Temperature is the threshold at which printing can begin without user intervention. Both values are included in the exported FPS. Verify your resin manufacturer’s recommendations and the printer’s supported temperature range.

Important: Choose a factory FPS template with the same layer thickness you intend to use. This tool edits supported exposure fields; it does not convert the underlying material or machine configuration.

Step 3 · Calculate & export — Studio 1 exposure settings

The Math Behind the Numbers

These calculations estimate the UV exposure dose for a third-party resin using the source printer's irradiance and exposure time. The values below update automatically when you change the inputs in Step 2.

1. Exposure energy

E = I × t

E = exposure energy (mJ/cm²); I = UV irradiance (mW/cm²); t = exposure time (seconds). Since 1 mW = 1 mJ/s, multiplying irradiance by time gives energy per unit area.

2. Converting exposure between printers

Etarget = Isource × tsource × C
tStudio 1 = Etarget / IStudio 1

C is the adjustable calibration factor. A value of 1.00 means no dose correction; it does not guarantee matching cure behavior. The generator writes the estimated dose in mJ/cm² to the Studio 1 FPS profile; the equivalent exposure time shown here is for understanding the conversion.

3. Your live calculation

Enter valid source settings to see the calculation.

4. Other generated values

Touchpoint exposure = target dose × touchpoint ratio. The initial early-layer exposure values are adjustable separately and transition toward the target normal dose. Bottom exposure and transition-layer counts are shown as reference diagnostics; they are not transferred directly as identical settings between printers.

Important limitation: Equal calculated UV energy does not guarantee identical curing behavior across different printers. Wavelength, optical system, exposure uniformity, resin chemistry, and printing conditions can affect the results. Always validate the generated profile with calibration prints.

Nominal M7 normal dose
—
mJ/cm²
Corrected Studio 1 normal dose
—
mJ/cm²
Studio 1 theoretical exposure time
—
seconds at selected irradiance

Review the calculated values before exporting. Operating and start temperatures are exported to the FPS using the selected resin temperature. These are estimates, not validated cure settings. You can fine-tune the calibration parameters in Step 4 below, then return here to export an updated FPS.

PreForm fieldSuggested value
Reference / diagnosticsValue
Source bottom-layer energy is an irradiance × exposure-time estimate only. It is NOT converted into a Studio 1 bottom-layer setting. Studio 1 initial-layer exposure follows the separate early-layer curve in Step 4; calibrate it independently.

Normal/Perimeter/Supports/Top dose are mapped together for initial testing. Touchpoints use the adjustable Alpha Grey ratio. Overhang Fill Exposure is intentionally left unchanged pending inspection of its array.

Profile safety checks

Live checks flag unusual values. A passed check does not mean the resin or generated profile has been physically validated.

Enter settings to see checks.

Operating and Start Temperature must each be between 0 and 45 °C. Export is disabled outside this range.

Before exporting, the tool also verifies that only intended FPS fields have changed.

Step 4 · Calibrate — Results & adjustments

Calibrate your profile in one place: plan a test, assess the results, adjust exposure and adhesion settings, and keep a record of each print. Expand a section below to work through the process.

Calibration sweep & test resources

Suggested test doses around the corrected target. Print separate small calibration pieces; inspect fine holes, thin walls, support retention and overcure. These are not validated material settings.

Need a calibration test model?

All3DP has a collection of resin printer test prints, with guidance on what to look for when evaluating the results. Choose a small test that matches the detail or adhesion issue you want to investigate, then use the calibration sweep below to compare exposure doses.

Browse resin calibration prints and evaluation tips on All3DP ↗

External resource. Download models from their respective sources and follow the model creator’s instructions; these are not Studio 1-validated settings.

Print failed? Check your printer before trying again.

If a calibration print fails, do not immediately start another print. Inspect the resin tank and build platform for failed parts, cured resin, or debris. Remove any remaining material using the appropriate cleaning procedure before continuing.

Formlabs guide: Cleaning a failed print with the Cleaning Sheet (Form Studio 1) ↗
TestDose (mJ/cm²)Equivalent Studio time (s)
Calibration results & history

Print feature assessment

Print feature assessment · Optional

Mark what passed and what failed on the same calibration print. Leave anything you could not evaluate unchecked. Recommendations are diagnostic starting points, not automatic proof of an exposure problem.

Small features / fine details
Large / solid features
Overhangs
Supports / touchpoints
Build platform adhesion
Holes / negative details

A failed feature does not uniquely identify its cause. Check orientation, supports, washing, peel behavior and resin condition before changing settings. If a print failed, inspect and clean the tank before retrying.

Record successful or failed tests in your browser. Assess the print below, review editable adjustments in a popup, then record the result and A → B changes in Test notes. History is stored locally in this browser.

DateResin / doseResult / notes
Dose mapping & profile adjustment

Optional advanced tuning: after a test print, adjust the correction factor and support touchpoint ratio. Changes update the calculated settings in Step 3 automatically.

After a successful calibration, enter the best-performing Studio 1 dose. The calculator sets k = best dose ÷ nominal M7 normal dose. This is an empirical correction for this resin, thickness and setup—not a universal optical conversion.

Early-layer exposure curves

Three Studio 1 control points are linearly interpolated by height. Early-layer values initially follow the imported FPS profile when available; the final point follows the corrected normal dose. Imported early-layer doses are inherited from the template and are not validated for your third-party resin.

Exposure dose (mJ/cm²) vs. height (mm): imported FPS vs. proposed profile
Interpolated Studio 1 early-layer doses by layer index
HeightExposureOffsetIrradiance
Troubleshooting guide

Use the observed failure pattern to decide what to inspect first. Change one variable at a time, record the result, and inspect the resin tank and build platform after any failed print. These are diagnostic suggestions, not guaranteed fixes.

Nothing adheres to the build platform: verify that a compatible Resin Tank Pro is installed, the build platform is correctly seated and locked, and the resin is mixed and at the recommended temperature. Inspect the tank for cured debris or damaged film. If hardware and preparation are sound, compare the imported early-layer exposure curve with your test results; adjust early-layer adhesion settings in small increments rather than increasing normal exposure indiscriminately.

Raft adheres, but supports detach or the model separates: determine whether the failure occurs at the support base, along support shafts, or at touchpoints. Check support density, tip diameter, model orientation, suction/cross-sectional area, and peel forces. If touchpoints are specifically failing while model detail is acceptable, consider a small touchpoint-dose adjustment and retest; increasing overall model exposure may unnecessarily close fine details.

Fine details disappear or small holes close: compare positive and negative details on the calibration model. Overexposure can broaden cured features and close openings. Check that the model was not overwashed, swollen, or overcured during post-processing. If the effect is repeatable across orientations, test a slightly lower normal dose while leaving early-layer settings unchanged.

Thin features are missing or surfaces look undercured: check whether small pins, text, or unsupported edges are consistently incomplete. Confirm the resin was mixed, the temperature is suitable, and the source irradiance/exposure inputs are correct. Try a small normal-dose increase only after excluding orientation and support limitations; inspect whether holes begin to close as a trade-off.

Overhangs warp, curl, or fail: check orientation, support placement, local cross-sectional area, drainage/venting and peel forces before changing dose. Compare supported and unsupported overhangs. A higher exposure dose is not a universal solution for mechanical distortion or suction-related failures.

Layer separation, delamination, or inconsistent results: inspect the tank film, resin condition and temperature, build-platform seating, and whether large cross-sections or trapped volumes increase peel forces. Repeat a small controlled test before modifying multiple exposure settings.

Print failure or debris in the tank: stop before launching another print. Inspect the tank and build platform for detached or cured material and follow the official Form Studio 1 Cleaning Sheet procedure when appropriate. Never scrape or continue printing over loose cured fragments.

Hardware reminder: Use a compatible Resin Tank Pro for third-party resins. Check compatible accessories.

Saved presets · Optional

Enter or edit the preset name before saving. Saving under a new name creates a separate preset; an existing name will ask before overwriting. Presets are stored locally in this browser, not as FPS files.

Review calibration adjustments

These are experimental suggestions based on the selected print observations, not diagnoses. Edit the proposed values before applying. No changes are made until you confirm.

Only checked and edited values will update Step 3. Confirm the hardware, support geometry, and tank condition before printing again.

Before using Resin Profile Lab

This independent community tool generates experimental print settings. It is not affiliated with or endorsed by Formlabs or Anycubic.

Required hardware: Use a Resin Tank Pro for third-party resin on the Form Studio 1. An incompatible tank may cause failed prints or damage. Formlabs compatible accessories ↗

Risks: Generated profiles are estimates and are provided “as is” without warranties. Incorrect settings may cause print failures, resin spills, damage to the printer or components, and other losses. Inspect the printer after a failed print and calibrate before production use.

Responsibility and liability: You are responsible for verifying the settings, confirming hardware compatibility, and deciding whether to print. To the fullest extent permitted by applicable law, the developer disclaims liability for damage, injury, costs, claims, or losses arising from use of the tool or generated profiles. This does not exclude liability that cannot lawfully be excluded.

Export your custom FPS

Give the new profile a clear name. Your original factory FPS is not overwritten.

Need a Resin Tank Pro? View compatible accessories in the Formlabs webshop ↗